Ameralloy® Oil OIL HARDENING AISI 0-1

Ameralloy Oil is the most widely used grade of drill rod. It is a general purpose tool steel with premium hardening, wear resistance, and toughness.

Ameralloy® -60 AIR HARDENING AISI A-6

Ameralloy-60 has a minimum distortion characteristic which makes it particularly well suited for dies and punches in blanking and forming operations.

Typical Analysis GENERAL PURPOSE

  • Carbon .90
  • Manganese 1.20
  • Silicon .30
  • Tungsten .55
  • Chromium .65
  • Vanadium .30
  • Molybdenum .15

Typical Analysis

  • Carbon .70
  • Molybdenum .09
  • Manganese 2.10
  • Silicon .30
  • Chromium 1.00
  • Vanadium 1.35

Ameralloy® -Air AIR HARDENING AISI A-2

Ameralloy Air is recommended over Ameralloy Oil when increased wear resistance, safe hardening, and less distortion are required.

Ameralloy® D-2 HIGH CARBON/
HIGH CHROME AISI D-2

Ameralloy D-2 is an air-hardening steel known for maximum wear resistance. It is ideal for use in tools, dies, and used in long production runs.

Typical Analysis MINIMUM DISTORTION

  • Carbon 1.00
  • Molybdenum 1.15
  • Manganese .60
  • Silicon .20
  • Chromium 5.75
  • Vanadium .25

Typical Analysis MAX. WEAR RESISTANCE

  • Carbon 1.55
  • Molybdenum 1.00
  • Manganese .55
  • Silicon .35
  • Chromium 12.50
  • Vanadium 1.00

Typical Analysis

  • Carbon .18
  • Manganese .50
  • Silicon .20
  • Phosphorus .04
  • Sulphur .04

Typical Analysis

  • Thickness +.005, -.000 Mattison ground
  • Width +.005, -.000 Blanchard ground
  • Length plus 1/8” saw cut
  • Heat treated to 28–32 Rockwell C

Ameralloy® -7 SUPER SHOCK AISI S-72

Ameralloy-7 is our new, premium quality air hardening drill rod. It’s the toughest, strongest drill rod for many applications that require maximum strength and impact.

High Speed-2 HOT WORK AISI M-2

Ameralloy High Speed-2 is the most widely used type of high speed tool steel. It’s higher carbon content and balanced analysis produce ideal properties for high speed use.

Typical Analysis MAXIMUM STRENGTH

  • Carbon .50
  • Molybdenum 1.40
  • Manganese .70
  • Silicon .25
  • Chromium 3.25

Typical Analysis

  • Carbon .86
  • Molybdenum 5.00
  • Tungsten 6.35
  • Chromium 4.15
  • Vanadium 1.90